Abstract

To compare gloss retention of four different resin composites with their corresponding CAD/CAM composite blocks.

Four direct resin composites (Filtek Supreme XTE A2 Body (3M, USA), Tetric EvoCeram A2 (Ivoclar Vivadent, Liechtenstein), GrandioSO x-tra A2 (VOCO, Germany), G-aenial Universal A2 (GC, Japan)), and their corresponding CAD/CAM composite blocks were tested. A total of 288 samples were prepared and three different tests were performed: brushing, exposition to acidic fluoride gel and exposition to alcoholic solution. Gloss values were obtained by means of a glossmeter at T0 before aging and T60 after 1 h of aging.

Mean gloss values ranged from 0.9 after brushing tests to 79.0 after the alcohol test witnessing a high gloss variability depending on the materials and the aging test. Statistical analysis by means of two-way repeated measures ANOVA followed by Fisher's LSD post-hoc test revealed significant differences between materials, storage media, and their interactions.

Gloss retention seems to be dependent on the composite type (direct or CAD/CAM block) and composite brand and varies in respect to the type of aging. CAD/CAM materials showed a higher resistance toward alcohol exposure.

eng
Keywords
  • CAD/CAM
  • Gloss resin composite
Citation (ISO format)
ARDU, Stefano et al. Gloss retention of direct composites and corresponding CAD/CAM composite blocks. In: Clinical and experimental dental research, 2021. doi: 10.1002/cre2.505
Main files (1)
Article (Published version)
Identifiers
ISSN of the journal2057-4347
156views
177downloads

Technical informations

Creation10/19/2021 10:51:00 AM
First validation10/19/2021 10:51:00 AM
Update time03/16/2023 1:35:12 AM
Status update03/16/2023 1:35:11 AM
Last indexation05/06/2024 8:20:54 AM
All rights reserved by Archive ouverte UNIGE and the University of GenevaunigeBlack